How to do a second pour?

A second pour fills the sink hole that forms on cooling, with the same recipe. Why it sank is in a separate guide. Soya Wax 50 ~51–55°C; do not add fragrance or exceed the first load. Do not bury the wick; tip ~5 mm.

  1. Wait for the first layer

    The surface should be solid to the touch. Pouring while warm slides the layer. The sinking cause is in a separate article.

  2. Melt the same wax

    Soya Wax 50 double boiler ~51–55°C. Do not add new fragrance; oil saturation ~8%. For paraffin, the SKU temperature.

  3. Fill the hole

    A thin stream, do not bury the wick. Cool it, tip ~5 mm. Bubbles are a separate guide.

Not the cause

Fast cooling and air pockets are in the why-does-a-candle-sink article. This page is only filling.

Mold

A second pour in a candlestick mold is for the surface hole. Early demolding bending is separate.

FAQs

Can a different scent be added?

No. The same lot. New fragrance causes sweating.

How many times?

One thin layer is enough. Thick layers on top bury the wick.